If you have this type of siding and it is stained consider not painting.
Painting house siding cracked plywood.
Painting t 111 siding requires a lot of work and paint.
Repair any holes or deep cracks in the siding with an epoxy filler formulated for wood.
Also check to be sure you ve covered all areas with paint.
This type of siding is very difficult to keep painted due to all the cracks in the plywood that develop over time.
Sand 3 inches past the end of the crack.
Tools and materials for painting t1 11 siding.
This allows for the caulk to get in and fill the gap correctly.
Painting t 111 takes time but ensuring a proper coat of paint.
Cracking stained rough strewn siding thin long relatively straight cracks running in a singular direction on a previously stained wood surface.
Restaining t 111 siding is a good alternative to paint.
Apply with a putty knife smoothing the top of the patch.
How to use caulk and water to fill in cracks in the worn siding before painting.
Ladder if applicable wire brush.
Cracks and imperfections abound in plywood based siding such as t 111 and this makes painting more difficult then other siding types.
Sometimes the old caulk in the siding joint is cracked and you need to cut the old caulk out with a razor knife.
According to the centers for disease control cdc lead paint should be removed by contractors who are certified by the epa.
T 111 wood siding requires paint to provide an adequate barrier against moisture damage to your home.
Brush or broom to clean up scrapings.
Cracking plywood checking thin long and relatively straight cracks that form in the paint film usually in the direction of the plywood grain.
Use long horizontal strokes with the block instead of short vertical strokes.
Work a paint scraper from every direction keeping the blade flat against the wood so you don t create gouge marks.
Basically any crack on the exterior of the house should be filled.
Once the second coat has dried completely inspect the siding for any cracks or small holes you may have overlooked.
Cracks and holes in any surface collect water which causes paint to peel.
If the siding joint is so tight that the caulk only bridges the gap it may split again.
Wipe with a tack cloth to remove all dust before priming and painting.
Sand the surface of the siding at the area of the crack with a sanding block.